Rims fused aluminum alloy more used is GK AlSi7Mg
After obtaining the proper preform heating is necessary to ensure sufficient ductility in flowforming. At the same time, it is necessary to heat the mold to prevent cooling of the rim during the process. |
|
The flowforming process is realized on longer wing fused in the outline. After flowforming the micro grain is compacted and flowformed, so the hardness of the flowforming wing is increased. At the same time the thickness wing can be reduced from 4.0-6.0 to 2.5-3.0 mm. approx. |
|
The process is carried out with the range of flowforming vertical lathes DENN LW3-180 y 245 CNC, three rollers with independent working three cars specifically designed for this application. |
Thanks to powerful software programming DENN CAD-CAM get the best optimization of process in fast, easy and intuitive. |
 |
DENN's process department process will provide a personalized study according to your needs. |
 |
DENN CAD-CAM |
|